Nitronic 60 is an anti-galling and wear resistant stainless steel.
Nitronic 60 is also known as Alloy 218 and HPA 50.
Chemical Composition | Specifications | Designations | Key Features | Typical Applications | ||||||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
|
AMS 5848 ASTM A580 |
UNS S21800 AWS 166 |
Anti galling Wear resistant |
Valve Stems Pins Brushes Roller bearings Pump shafts and rings Thread inserts Fasteners |
Density | 7.6 g/cm³ | 0.28 lb/in³ |
Melting Point | 1375°C | 2500°F |
Coefficient of Expansion | 15.8 μm/m °C (21 – 200°C) | 8.810 x 10-6 in/in °F (70 – 212°F) |
Modulus of Rigidity | 69 kN/mm² | 10008 ksi |
Modulus of Elasticity | 181 kN/mm² | 26200 ksi |
Heat Treatment of Finished Parts | |||||
---|---|---|---|---|---|
Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
°C | °F | ||||
Annealed or Spring Temper | Stress Relieve | 250 | 480 | 1 | Air |
Properties | ||||
---|---|---|---|---|
Condition | Approx. tensile strength | Approx. operating temperature | ||
N/mm² | ksi | °C | °F | |
Solution Annealed | 700 – 1000 | 102 – 145 | -200 to +300 | -330 to +570 |
Spring Temper | 1300 – 1900 | 189 – 276 | -200 to +300 | -330 to +570 |
The above tensile strength ranges are typical. If you require different please ask.
*Trade name of AK Steel