MP35N is an age hardenable Nickel-Cobalt base alloy that has a unique combination of properties – ultra high strength, toughness, ductility and outstanding corrosion resistance. MP35N resists corrosion in hydrogen sulphide, salt water and other chloride solutions. It also has excellent resistance to crevice and stress corrosion cracking in sea water and other hostile environments. Suitable where a high combination of strength, high modulus values and good corrosion resistance are required. Applications for this alloy also include medical devices and dental products.
MP35N is also known as Allvac 35N.
Chemical Composition | Specifications | Designations | Key Features | Typical Applications | ||||||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
|
AMS 5844 AMS 5845 ASTM F562 ISO 15156-3 (NACE MR 0175) ISO 5832-6 |
W. Nr. 2.4999 UNS R30035 AWS 110 |
Combination of high strength, ductility and good mechanical properties at ambient temperatures Excellent corrosion resistance in hydrogen sulphide Excellent resistance to crevice and stress corrosion cracking in sea water Age hardenable (Spring Temper only) |
Medical Devices Marine Engineering |
Density | 8.43 g/cm³ | 0.304 lb/in³ |
Melting Point | 1440°C | 2625°F |
Coefficient of Expansion | 12.8 μm/m °C (20 – 100°C) | 7.1 x 10-6 in/in °F (70 – 212°F) |
Modulus of Rigidity | 80.7 kN/mm² | 11705 ksi |
Modulus of Elasticity | 234 kN/mm² | 33939 ksi |
Heat Treatment of Finished Parts | |||||
---|---|---|---|---|---|
Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
°C | °F | ||||
Annealed | – | – | – | – | – |
Spring Temper | Age Harden | 650 | 1200 | 4 | Air |
Properties | ||||
---|---|---|---|---|
Condition | Approx. tensile strength | Approx. operating temperature | ||
N/mm² | ksi | °C | °F | |
Annealed | < 1100 | < 160 | -200 to +315 | -330 to +600 |
Spring Temper | 1400 – 1900 | 203 – 276 | -200 to +315 | -330 to +600 |
Spring Temper + Aged | 1900 – 2200 | 276 – 319 | -200 to +315 | -330 to +600 |
The above tensile strength ranges are typical. If you require different please ask.
*Trade name of SPS Technologies